Liquid phase morphology control of ZnO crystals was realized with simple aqueous solution system. ZnO nanowires were successfully\r\nfabricated at 50?C. They were over 50 �µm in length and about 100nm in width. Aspect ratio was estimated to be over\r\n500. They had no branches and were obtained without aggregations. Curved nano-wires clearly indicated high flexibility and high\r\nmechanical strength. Additionally, ellipse particles, hexagonal rods and particles were fabricated in the solutions. Morphology,\r\ncrystal growth speed, and preferred growth faces were well-controlled by precise adjustment of growth conditions.